HiSupplier Escrow |
Place of origin: China (Mainland)
Brand name:Adv-ti
Material:titanium
Standard: ASTM B265,AMS4911, AMS4916
Technique:hot rolled
Application:heat exchanger
Grade:GR1 GR2 GR5
thickness:0.3-10mm
length:2000-8000mm
processing technique:titanium sponge —compacting electrode—melting—titanium ingots—forging—slab—hot rolling—hot-rolled sheets
Advantage:
Excellent corrosion resistance
strong oxidation resistance
long life time
non-magnetic
non-poisonous
high and low temperature resistance
small density
High tensile strength
Applications:
With the development of science and technology, the application field of titanium is becoming more and more broad, such as medical, automotive, sports, etc.
Through these application ,its good characteristics is more and more cognized and affirmed ,and integrate into our production applications instead of other metals with the fastest speed , even in our body.
Mechanical properties of titanium plate
(1)mechanical property at room temperature
Trade mark | Thickness(mm) | properties at room temperature,(no less than) | |||
Tensile Strength σbMPa | yield strength σ0.2MPa | elongation δ5% | Bending angle α degree(no less than) | ||
GR1 | 0.3~10.0 | 370-530 | 250 | 45-30 | 140-130 |
GR2 | 0.3~110.0 | 440~620 | 320 | 25 | 100-80 |
GR5 | 0.8~10.0 | 895 | 830 | 12-10 | 35-30 |
(2)Titanium plate temperature mechanical properties
surface quality:
1 The surface of the titanium plate should be smooth with its metal colour. The plate was permited to sand blasting with surface before delivery.
2 The surface was allowed with light darkness and water print in part ;local defects ,scratch,indentation and scallops with thickness less than half of the thickness was allowed ,but the minimum thickness should be ensured.
3 There should not be macro defects such as crack,peeling, oxide skin,backfin,and mixture with metal and non-metal.also should not be alkali washed too much.
4The plate was allowed to clear away the local defects along the direction of rolling ,but the thickness after clearness should not less than the minimum thickness allowed.
5In addition, the plate should not be delamination.